4 Causes of Flow Lines in Blown Film Extrusion (and One Easy Solution)

Flow lines are one of the most common processing issues faced by blown film extruders. There..

Read More


When Sheet Extruders Should Increase Heats While Purging (& When They Shouldn't)

I recently gave technical support to a new customer who is a Process Engineer at a mid-sized..

Read More


Expert Purging Tips for Your Top 5 Processing Headaches

I recently asked my customers to share with me what their Number 1 processing problem was. The..

Read More


5 Tips for Processing Heat-Sensitive Resins in Sheet Extrusion

Recently I performed a trial at a PVC sheet extruder who produces roofing. It took them 8-12..

Read More


Thickness Control for Sheet Extrusion

When extruding a flat sheet on a die we can have variations in thickness. Some variations can be..