The ASACLEAN Blog

Purging Compound Insights And Tips

Topic: Blown-film-purging

Failure Equals Success When Processing Post-Consumer Recycled Plastics (PCRs)

To paraphrase Thomas Edison when asked how it felt to fail at making a light bulb over 1000..

Read More



4 Causes of Flow Lines in Blown Film Extrusion (and One Easy Solution)

Flow lines are one of the most common processing issues faced by blown film extruders. There..

Read More


Make Sure The Purge You've Been Buying Still Makes Sense for Your Processing Needs

A large injection molding plant in the Southeast has been buying Asaclean Purging Compounds for..

Read More


How Back Pressure & Screw Speed Help Your Purge Perform

Back pressure is a huge factor in getting the most out of mechanical purging compounds.  It..

Read More


3 Injection Molding Tips for Shot-to-Shot Repeatability

For shot-to-shot repeatability there are many factors that play an important role and many test..

Read More


How to Achieve Cost Savings in Blown Film Extrusion

Plastics processors have different ways of measuring success when purging. Some care about..

Read More


How to Reduce Excess Hold Time in Injection Molding

Although your hold time is one of the most important stages of your cycle time, it is the one..

Read More


4 Tips:Reduce Residue in Clear Applications for Injection & Extrusion

   As most of you may know, when processing resins such as Polycarbonate, Acrylic, TPU or..

Read More


Removing Carbon in Blown Film Lines

Blown film extrusion processors deal with the same processing issues as everybody else. When..